Next: 20.2.1 Development of Strength
Up: 20. Time Effects on
Previous: 20.1.4 Shrinkage
Contents
Index
20.2 ACI 209 Model Code
The ACI 209 Model Code [1]
discerns cement types I and III and two curing methods:
with moist or with steam.
Table 20.2 gives the various coefficients to determine the
material properties.
Table 20.2:
COEFFICIENTS FOR ACI MODEL CODE
|
|
Cement type |
Curing |
duration |
|
|
|
I |
III |
|
ts
[days] |
|
Strength |
a
|
4.0 |
2.3 |
moist |
|
|
|
|
1.0 |
0.7 |
steam |
|
|
|
|
0.85 |
0.92 |
moist |
|
|
|
|
0.95 |
0.98 |
steam |
|
|
Shrinkage |
|
1.20 |
moist |
1 |
|
|
|
1.10 |
moist |
3 |
|
|
|
1.00 |
moist |
7 |
|
|
|
0.93 |
moist |
14 |
|
|
|
0.86 |
moist |
28 |
|
|
|
0.75 |
moist |
90 |